Welcome to our site! EDAboard.com is an international Electronics Discussion Forum focused on EDA software, circuits, schematics, books, theory, papers, asic, pld, 8051, DSP, Network, RF, Analog Design, PCB, Service Manuals... and a whole lot more! To participate you need to register. Registration is free. Click here to register now.

Recent content by smarty88

  1. S

    [SOLVED] Solder flaking and crumbling?

    Thanks so much, yes I have tried cleaning the component with flux prior and along with previous reply have concluded the cheaply purchased solder is of bad quality. I have a more expensive solder which works fine with or without additional flux, as soon as this solder is added to any existing or...
  2. S

    [SOLVED] Solder flaking and crumbling?

    Thanks Klaus, I appreciate your reply. I have tried to clean the component with flux prior, an the PCB i use is already tinned so it makes sense that there is most likely an issue with the cheap solder I have purchased. Appreciate your reply!
  3. S

    [SOLVED] Solder flaking and crumbling?

    I've been soldering for over 30 years and not experienced this problem before, bought some solder from ebay 60 tin/38 lead / 2 resin flux. also have another composition 63/37 supposedly with flux also. every time I add the solder to heated component and pcb pad it simply turns into flakes. no...