Welcome to our site! EDAboard.com is an international Electronics Discussion Forum focused on EDA software, circuits, schematics, books, theory, papers, asic, pld, 8051, DSP, Network, RF, Analog Design, PCB, Service Manuals... and a whole lot more! To participate you need to register. Registration is free. Click here to register now.

Need your kindly help: Why H2 alloy bring metal void ?

Status
Not open for further replies.

Dido_Huang

Newbie level 1
Joined
Apr 11, 2006
Messages
1
Helped
0
Reputation
0
Reaction score
0
Trophy points
1,281
Activity points
1,285
h2 alloy

In 0.18LG process, H2 alloy post metal etch will bring metal voids issue. Why?The temperature or the H2 cause it? Pls give me your comments,TKS.
 